Nanoindentation to Microhardness to Tensile Strength Correlation Coefficient Estimates in Relation to Microstructure in Eutectic Snbi Alloy

Nataliya Starostina

Determining strength to hardness correlation coefficients on nano and microscale in correspondence to microstructure and composition leads the way to inexpensive, non-destructive ways to predict tensile strength of bulk materials which is important for developing preventive maintenance procedures in the variety of industries. Nanohardness and microhardness tests were performed on an in-house prepared eutectic SnBi alloy. Elemental composition and eutectic morphology were verified by scanning electron microscopy and energy dispersive spectroscopy. Linear correlation coefficients, C1, between nanoindentation and Vickers microhardness, was determined based on experimental measurements and found to be greater than 1.25. Tabor factor, the ratio of Vickers microhardness to ultimate tensile strength, was estimated to be consistently greater than 3. Comparison to coefficients estimated from data available for other alloy systems is discussed.

免责声明: 此摘要通过人工智能工具翻译,尚未经过审核或验证

索引于

哥白尼索引
打开 J 门
学术钥匙
研究圣经
引用因子
宇宙IF
参考搜索
哈姆达大学
学者指导
国际创新期刊影响因子(IIJIF)
国际组织研究所 (I2OR)
宇宙
日内瓦医学教育与研究基金会
秘密搜索引擎实验室

查看更多